detail |
It is a two-component mixed component designed for the production of high-grade cold-cured high-rebound polyurethane foam products. The product performance is formulated according to the People's Republic of China industry standard QB/T2080-95. Component A consists of high-activity polyether polyol, surfactant, cross-linking agent, foaming agent and other components; component B is composed of isocyanate TDI, MDI, modified TDI. The operation is convenient and the product performance is superior.
Product list:
Brand
|
Product name
|
Scope of application
|
HW-0301
|
High density high rebound mixed component
|
Car, motorcycle, bicycle saddle
|
HW-0302
|
Medium density high rebound mixed component
|
Car, train, sofa cushion
|
HW-0303
|
Low density high rebound mixed component
|
Car, train, sofa seat back, toy
|
Physical properties:
Item\ Index\Component
|
Component A
|
Component B
|
Appearance
|
Milky white viscous liquid
|
Dark brown liquid
|
Specific gravity g/cm3
|
1.08±0.05
|
1.25±0.05
|
Viscosity CPS/25°C
|
1500±200
|
200±50
|
Hydroxyl value mgKOH/g
|
50±10
|
|
NCO %
|
|
35-46
|
Reaction time:
Item\Time S\ Model
|
HW-0301
|
HW-0302
|
HW-0303
|
Cream time
|
10-12
|
8-10
|
6-10
|
Gelation time
|
80-90
|
60-80
|
60-70
|
Demoulding time
|
200-300
|
200-240
|
180-240
|
Performance Index of Products:
Item\ Index\ Model
|
HW-0301
|
HW0302
|
HW-0303
|
Density Kg/m3
|
60-80
|
45-55
|
35-40
|
Tensile strength, Kpa≥
|
100
|
80
|
75
|
Elongation%≥
|
90
|
100
|
110
|
Rebound rate%≥
|
55
|
60
|
60
|
Tear strength N/cm≥
|
2.5
|
1.75
|
1.7
|
Maximum change rate of tensile strength after dry heat aging
(140 ° C, 16 h)
|
±30
|
±30
|
±30
|
Maximum change rate of tensile strength after damp heat aging
(105 ° C, 100% RH, 3 h)
|
±30
|
±30
|
±30
|
75% compression set
(70 ° C, 22h)% ≤
|
10
|
10
|
10
|
Hardness when indented 25%, N, ≥
|
180
|
120
|
120
|
Hardness when indented at 65%, N, ≥
|
468
|
315
|
315
|
65%/25% indentation ratio, ≥
|
2.6
|
2.6
|
2.6
|
Packing: galvanized barrel, 200KG / barrel
Storage: six months
|